Two streams of liquid metal, which are not hot enough to fuse properly, result into a casting defect known as

  1. cold shut

  2. swell

  3. sand wash

  4. scab

Reveal answer Fill a bubble to check yourself
A Correct answer
Explanation

Keep practicing — related questions

  • Match the casting defects (Group A) with the probable causes (Group B). | | | || |---|---|---|---| | |Group...
  • A mixture of water and salt makes metal ___.
  • accidentally touching a hot curling iron
  • When a solid is ________ to its melting point it becomes a liquid.
  • Laboratory tests revealed [a]that the metal using in[b] this particular model [c]was actually an alloy of i...
  • Laboratory tests revealed [a]/that the metal using in[b]/ this particular model[c]/ was actually an alloy o...
  • The hot tearing in a metal casting is due to
  • The two dissimilar metals are bonded with the process of
Play the full quiz 🎤 Practise this topic out loud

Practice this topic

  • Metallurgical Processes (1403 questions)
Advertisement
© Aliensbrain | all rights reserved
  • About
  • Contact
  • Terms and Condition
  • Privacy Policy