In Ostwald's process, Ammonia is converted to nitric acid in two stages. It is oxidized by heating with oxygen in the presence of a catalyst of platinum with 10% rhodium, to form nitric oxide and water. This step is stongly exothermic, making it a useful heat source once initiated (delta H = -950 kJ).